This standard practice determines application quantities for applying aggregate and emulsified asphalt for scrub seals.
A scrub seal is a four-step process in which the application of emulsified asphalt is followed immediately by a scrub broom to push the emulsion into the cracks in the pavement, followed with an application of a single layer of cover aggregate, and then rolled with a pneumatic tire compactor. There is the option of including a fog seal to help with chip retention.
Standard Method of Test for Portland-Cement Content of Hardened Hydraulic-Cement Concrete (ASTM Designation: C1084-02)
$21.00 $42.00
Standard Method of Test for Flexural Strength of Concrete (Using Simple Beam with Center-Point Loading) (ASTM Designation: C 293-08)
$18.00 $37.00
Standard Method of Test for Compressive Strength of Hot Mix Asphalt
$39.00 $78.00
Standard Method of Test for Bulk Specific Gravity of Compacted Hot Mix Asphalt (HMA) Using Saturated Surface-Dry Specimens