These methods of test cover procedures for determining the soil–cement losses, moisture changes, and volume changes (swell and shrinkage) produced by the repeated wetting and drying of hardened soil–cement specimens. The specimens are compacted in a mold, before cement hydration, to maximum density at optimum moisture content using the compaction procedure described in AASHTO T 134.
Two methods, depending on soil gradation, are covered for preparation of material for molding specimens and for molding specimens as follows:
Standard Method of Test for Evaluation of the Tracking Resistance of Hot-Poured Asphalt Crack Sealant by Dynamic Shear Rheometer (DSR)
$39.00 $78.00
Standard Practice for Pipe Joint Selection for Highway Culvert and Storm Drains
$44.00 $89.00
Standard Method of Test for Measuring Adhesion of Hot-Poured Asphalt Crack Sealant Using Direct Adhesion Tester
Standard Specification for Steel Wire and Welded Wire, Plain and Deformed, for Concrete Reinforcement