• AASHTO T 324-11

AASHTO T 324-11

Standard Method of Test for Hamburg Wheel-Track Testing of Compacted Hot Mix Asphalt (HMA)

American Association of State and Highway Transportation Officials, 2011

Publisher: AASHTO

File Format: PDF

$25.00$50.00


Pages:10

File Size:1 file , 1.9 MB

Note:This product is unavailable in Ukraine, Russia, Belarus

This test method describes a procedure for testing the rutting and moisture-susceptibility of hot mix asphalt (HMA) pavement samples in the Hamburg Wheel-Tracking Device.

The method describes the testing of submerged, compacted HMA in a reciprocating rolling-wheel device. This test provides information about the rate of permanent deformation from a moving, concentrated load. A laboratory compactor has been designed to prepare slab specimens. Also, the Superpave© Gyratory Compactor (SGC) has been designed to compact specimens in the laboratory. Alternatively, field cores of diameter 150 mm (6 in.), 250 mm (10 in.), or 300 mm (12 in.), or saw-cut slab specimens may be tested.

The test method is used to determine the premature failure susceptibility of HMA due to weakness in the aggregate structure, inadequate binder stiffness, or moisture damage. This test method measures the rut depth and number of passes to failure.

The potential for moisture damage effects are evaluated because the specimens are submerged in temperature-controlled water during loading.

More AASHTO standard pdf

AASHTO T 72-22

AASHTO T 72-22

Standard Method of Test for Saybolt Viscosity

$49.00 $99.00

AASHTO R 101-22

AASHTO R 101-22

Standard Practice for Developing Performance Engineered Concrete Pavement Mixtures

$49.00 $99.00

AASHTO MP 46-22

AASHTO MP 46-22

Standard Specification for Balanced Mix Design

$49.00 $99.00

AASHTO PP 95-22

AASHTO PP 95-22

Standard Practice for Preparation of Indirect Tension Performance Test Specimens

$43.00 $86.00