• AASHTO T 99-18

AASHTO T 99-18

Standard Method of Test for Moisture-Density Relations of Soils Using a 2.5-kg (5.5-lb) Rammer and a 305-mm (12-in.) Drop

American Association of State and Highway Transportation Officials, 2018

Publisher: AASHTO

File Format: PDF

$48.00$96.00


Pages:14

File Size:1 file , 1.3 MB

Note:This product is unavailable in Ukraine, Russia, Belarus

These methods of test are intended for determining the relation between the moisture content and density of soils compacted in a mold of a given size with a 2.5-kg (5.5-lb) rammer dropped from a height of 305 mm (12 in.). Four alternate procedures are provided as follows:

  • Method A—A 101.60-mm (4-in.) mold: Soil material passing a 4.75-mm (No. 4) sieve
  • Method B—A 152.40-mm (6-in.) mold: Soil material passing a 4.75-mm (No. 4) sieve
  • Method C—A 101.60-mm (4-in.) mold: Soil material passing a 19.0-mm (3/4-in.) sieve
  • Method D—A 152.40-mm (6-in.) mold: Soil material passing a 19.0-mm (3/4-in.) sieve

The method to be used should be indicated in the specifications for the material being tested. If no method is specified, the provisions of Method A shall govern.

This test method applies to soil mixtures that have 40 percent or less retained on the 4.75-mm (No. 4) sieve, when Method A or B is used and 30 percent or less retained on the 19.0-mm (3/4-in.) sieve, when Method C or D is used. Material retained on these sieves shall be defined as oversized particles (coarse particles).

If the test specimen contains oversized particles, dry density and moisture corrections must be made in accordance with Annex A1. The person or agency specifying this method may specify a minimum percentage of oversized particles above which a correction must be applied. If no minimum percentage is specified, correction for the oversized particles shall be applied to material containing more than 5 percent by weight of oversized particles.

If the specified oversized particle maximum percentage is exceeded, other methods of compaction control must be used.

Note—One method for the design and control of the compaction of such soils is to use a test fill to determine the required degree of compaction and a method to obtain that compaction. Then use a method specification to control the compaction by specifying the type and size of compaction equipment, the lift thickness, and the number of passes.

AASHTO T 99-18 history

AASHTO T 99-18

AASHTO T 99-18

Standard Method of Test for Moisture-Density Relations of Soils Using a 2.5-kg (5.5-lb) Rammer and a 305-mm (12-in.) Drop

$48.00 $96.00

More AASHTO standard pdf

AASHTO T 272-18 (2022)

AASHTO T 272-18 (2022)

Standard Method of Test for One-Point Method for Determining Maximum Dry Density and Optimum Moisture

$39.00 $78.00

AASHTO T 383-18

AASHTO T 383-18

Standard Method of Test for Evaluation of Asphalt Release Agents (ARAs)

$44.00 $89.00

AASHTO T 355-18

AASHTO T 355-18

Standard Method of Test for In-Place Density of Asphalt Mixtures by Nuclear Methods

$44.00 $89.00

AASHTO R 91-18 (2022)

AASHTO R 91-18 (2022)

Standard Practice for Determining Aggregate Source Shape Values from Digital Image Analysis Shape Properties

$44.00 $89.00