Description: Question: What does it mean when a packaged repair material is labeled as shrinkage-compensating or nonshrink?

Answer: The terms 'shrinkage-compensating' and 'nonshrink' are both intended to describe materials that exhibit no or little net contraction as a result of shrinkage. In practice, however, these terms are of limited use in the selection of repair materials without supporting test data on time-dependent volume changes.

ACI 364.15T-18 history

ACI 364.15T-18

ACI 364.15T-18

TechNote: Significance of the Shrinkage-Compensating and Nonshrink Labels on Packaged Repair Materials

$9.00 $19.00

More ACI standard pdf

ACI MCP614

ACI MCP614

Manual of Concrete Practice Part 6 (2014)

$108.00 $217.25

ACI 550.3M-13

ACI 550.3M-13

Design Specification for Unbonded Post-tensioned Precast Concrete SPecial Moment Frames Satisfying ACI 374.1 (ACI 550.3-13) and Commentary

$36.00 $73.50

ACI 349M-13

ACI 349M-13

Code Requirements for Nuclear Safety-Related Concrete Structures and Commentary (Metric)

$75.00 $151.50

ACI 506.2-13 (R2018)

ACI 506.2-13 (R2018)

Specification for Shotcrete

$27.00 $54.50