1.1 This test method covers the determination of the weight and composition of coating on terne sheet by the triple-spot method. The following three procedures are described:
1.1.1 Procedure A - Stripping with sulfuric acid.
1.1.2 Procedure D - Stripping with hydrochloric acid and antimony trichloride.
1.1.3 Procedure E - Stripping with hydrobromic acid-bromine solution.
1.2 If the percent of tin in the coating is required, stripping with hydrobromic acid-bromine is the preferred procedure. Steel with a predeposited electrolytic nickel coating requires a two-stage stripping method to determine total tin content. If both the tin and lead percentage are required, stripping with sulfuric acid is recommended, but caution is advised since the sulfuric acid procedure has been found to produce high tin results (see Section 11).
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. For specific hazards statements, see Section 5, Note 2, and Section 17.
Standard Specification for Magnesium-Alloy Sheet and Plate
$30.00 $60.00
Standard Test Method for Total Energy Impact of Plastic Films By Dart Drop
Standard Test Method for Tensile Stress-Strain of Carbon and Graphite
$33.00 $67.00
Standard Test Methods for Fully Cured Silicone Rubber-Coated Glass Fabric and Tapes for Electrical Insulation (Withdrawn 2019)