• ASTM A576-17

ASTM A576-17

Standard Specification for Steel Bars, Carbon, Hot-Wrought, Special Quality

ASTM International, 11/01/2017

Publisher: ASTM

File Format: PDF

$24.00$48.00


Published:01/11/2017

Pages:6

File Size:1 file , 81 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers hot-wrought special quality carbon steel bars. Special quality bar applications include forging, heat treating, cold drawing, machining, and many structural uses. A guide for the selection of steel bars is contained in Practice A400.

1.2 The bars shall be furnished in the grades specified in Table 1. Sections and sizes of bar steel available are covered in Specification A29/A29M. Hot-wrought special quality carbon steel bars are produced in cut lengths and coils; the manufacturer should be consulted regarding sections and sizes available in coils, produced to a chemical composition.

Rephosphorized and Resulfurized Carbon SteelE, G, H

Designation

Grade

Carbon

Manganese

Phosphorus

Sulfur

Lead

G12110

1211

0.13 max

0.60-0.90

0.07-0.12

0.10-0.15

...

G12120

1212

0.13 max

0.70-1.00

0.07-0.12

0.16-0.23

...

G12130

1213

0.13 max

0.70-1.00

0.07-0.12

0.24-0.33

...

G12150

1215

0.09 max

0.75-1.05

0.04-0.09

0.26-0.35

...

...

12L14

0.15 max

0.85-1.15

0.04-0.09

0.26-0.35

0.15-0.35

(A) New designations established in accordance with Practice E527 and SAE J 1086.
(B) Maximum unless otherwise indicated.
(C) When silicon is required, the following ranges and limits are commonly specified: 0.10 %, max, 0.10 to 0.20 %, 0.15 to 0.35 %, or 0.20 to 0.40 %.
(D) Copper can be specified when required as 0.20 % minimum.
(E) When lead is required as an added element to a standard steel, a range of 0.15 to 0.35 % incl is specified. Such a steel is identified by inserting the letter “L” between the second and third numerals of the grade designation, for example, 10 L 45. A cast or heat analysis is not determinable when lead is added to the ladle stream.
ASTM E1316-18

ASTM E1316-18

Standard Terminology for Nondestructive Examinations

$41.00 $83.00

ASTM E2469-16

ASTM E2469-16

Standard Test Method for Chloride in Mono-, Di- and Tri-ethylene Glycol by Ion Chromatography

$25.00 $50.00

ASTM D4171-16a

ASTM D4171-16a

Standard Specification for Fuel System Icing Inhibitors

$31.00 $62.00

ASTM D4698-21

ASTM D4698-21

Standard Practice for Total Digestion of Sediment Samples for Chemical Analysis of Various Metals

$27.00 $54.00