1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.

1.2 The grades of high alloys detailed in Table 1 are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.

1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.

1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of each other. Combining values from the two systems may result in nonconformance with the specification.

More ASTM standard pdf

ASTM F1931-98(2004)

ASTM F1931-98(2004)

Standard Test Method for Characterization of Gymnastic Landing Mats and Floor Exercise Surfaces (Withdrawn 2011)

$25.00 $50.00

ASTM E379-68(1981)e1

ASTM E379-68(1981)e1

Specification for Apparatus for Direct Microdetermination of Oxygen in Organic Compounds

$120.00 $240.47

ASTM C549-81(1986)

ASTM C549-81(1986)

Standard Specification for Perlite Loose Fill Insulation

$30.00 $60.00

ASTM D7823-13

ASTM D7823-13

Standard Test Method for Determination of Low Level, Regulated Phthalates in Poly (Vinyl Chloride) Plastics by Thermal Desorption -- Gas Chromatography/Mass Chromatography

$32.00 $65.00