• ASTM A608/A608M-06

ASTM A608/A608M-06

Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperature

ASTM International, 09/01/2006

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:01/09/2006

Pages:6

File Size:1 file , 89 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.

1.2 The grades of high alloys detailed in are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.

1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.

1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of each other. Combining values from the two systems may result in nonconformance with the specification.

More ASTM standard pdf

ASTM D4538-95

ASTM D4538-95

Standard Terminology Relating to Protective Coating and Lining Work for Power Generation Facilities

$25.00 $50.00

ASTM F1599-95(2003)

ASTM F1599-95(2003)

Standard Guide for Collecting Performance Data on Temporary Storage Devices

$29.00 $58.00

ASTM D808-16

ASTM D808-16

Standard Test Method for Chlorine in New and Used Petroleum Products (High Pressure Decomposition Device Method) (Withdrawn 2021)

$32.00 $64.00

ASTM F1500-98(2003)

ASTM F1500-98(2003)

Standard Test Method for Quantitating Non-UV-Absorbing Nonvolatile Extractables from Microwave Susceptors Utilizing Solvents as Food Simulants

$25.00 $50.00