This specification covers the standard for iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures. The tubing shall be supplied in the as cast condition or as cast with machining on the outside or inside surfaces. The material shall conform to the required chemical composition in carbon, manganese, silicon, chromium, nickel, phosphorus, sulfur, and molybdenum. Tension test shall be performed in the tubing at elevated temperature and shall conform to the required values in tensile strength and elongation. Tubing shall meet several tests such as; pressure test, flattening test, and mechanical test.

More ASTM standard pdf

ASTM F2519-05(2015)

ASTM F2519-05(2015)

Standard Test Method for Grease Particle Capture Efficiency of Commercial Kitchen Filters and Extractors

$44.00 $89.00

ASTM D2693-07(2012)

ASTM D2693-07(2012)

Standard Specification for Ethylene Glycol (Withdrawn 2021)

$28.00 $56.00

ASTM D6458-12

ASTM D6458-12

Standard Tables of Body Measurements for Boys, Sizes 8 to 14 Slim and 8 to 20 Regular

$33.00 $67.00

ASTM G65-15

ASTM G65-15

Standard Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus

$32.00 $65.00