1.1 This specification covers structural quality alloy steel plates.

1.2 The plates are usually specified to chemical composition requirements, but tensile properties may also be specified.

1.2.1 When tensile properties are required, the specific requirements must be compatible with the chemical composition, condition, and plate thickness.

1.3 The plates are available in the following four conditions:

1.3.1 Condition AR-As rolled (hot rolled),

1.3.2 Condition A-Annealed,

1.3.3 Condition N-Normalized, and

1.3.4 Condition NT-Normalized and tempered.

1.4 The plates are available in the following three forms:

1.4.1 Form I-Rectangular,

1.4.2 Form II-Circular and semi-circular, and

1.4.3 Form III-Sketch, including rings.

1.5 The plates are available in the following five edge categories:

1.5.1 Edge 1-Mill edge,

1.5.2 Edge 2-Universal mill edge,

1.5.3 Edge 3-Sheared edge,

1.5.4 Edge 4-Gas cut edge, and

1.5.5 Edge 5-Special cut edge.

1.6 The plates are available in the following seven finishes:

1.6.1 Finish 1-As rolled (hot rolled),

1.6.2 Finish 2-Blast cleaned,

1.6.3 Finish 3-Blast cleaned and oiled,

1.6.4 Finish 4-Pickled,

1.6.5 Finish 5-Pickled and oiled,

1.6.6 Finish 6-Painted, one prime coat, and

1.6.7 Finish 7-Painted, one prime coat and one finish coat.

1.6.8 The plates are usually specified to have Finish 1.

1.7 Supplementary requirements are provided for additional requirements that may be specified on the order.

1.8 When the steel is to be welded, it is presupposed that a welding procedure suitable for the grade of steel and intended use or service will be utilized. See Appendix X3 of Specification A6/A6M for information on weldability.

1.9 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

More ASTM standard pdf

ASTM D1290-95(2002)

ASTM D1290-95(2002)

Standard Test Method for Sediment in Water-Emulsion Polishes by Centrifuge

$26.00 $52.00

ASTM D5779-95a(2001)

ASTM D5779-95a(2001)

Standard Test Method for Field Determination of Apparent Specific Gravity of Rock and Manmade Materials for Erosion Control

$26.00 $52.00

ASTM D5779-95a

ASTM D5779-95a

Standard Test Method for Field Determination of Apparent Specific Gravity of Rock and Manmade Materials for Erosion Control

$25.00 $50.00

ASTM F1662-95

ASTM F1662-95

Standard Test Method for Verifying the Specified Dielectric Withstand Voltage of a Member Switch

$27.00 $54.00