1.1 This specification covers a group of cast duplex stainless steels (austenitic/ferritic).
1.2 The duplex stainless steel alloys offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these alloys will develop a range of approximately 30 to 60 % ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics.
Note 1 - Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600ºF [315ºC].
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.3.1 Within the text, the SI units are shown in brackets.
More ASTM standard pdf
ASTM D7422-10a
Standard Test Method for Evaluation of Diesel Engine Oils in T-12 Exhaust Gas Recirculation Diesel Engine
$44.00 $89.00
ASTM E911-98
Standard Specification for Glass Stopcocks with Polytetrafluoroethylene (PTFE) Plugs
$25.00 $50.00
ASTM E2151-02(2010)
Standard Terminology of Guides for Specifying and Evaluating Performance of Single Family Attached and Detached Dwellings (Withdrawn 2019)
$25.00 $50.00