• ASTM A890/A890M-18a

ASTM A890/A890M-18a

Standard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application

ASTM International, 09/01/2018

Publisher: ASTM

File Format: PDF

$24.00$48.00


Published:01/09/2018

Pages:5

File Size:1 file , 79 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers a group of cast duplex stainless steels (austenitic/ferritic).

1.2 The duplex stainless steel alloys offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these alloys will develop a range of approximately 30 to 60 % ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics.

Note 1: Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600 °F [315 °C].

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

1.3.1 Within the text, the SI units are shown in brackets.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

More ASTM standard pdf

ASTM F883-13(2022)

ASTM F883-13(2022)

Standard Performance Specification for Padlocks

$30.00 $60.00

ASTM D7109-20

ASTM D7109-20

Standard Test Method for Shear Stability of Polymer-Containing Fluids Using a European Diesel Injector Apparatus at 30 Cycles and 90 Cycles

$30.00 $60.00

ASTM F3275-22

ASTM F3275-22

Standard Guide for Using a Force Tester to Evaluate Performance of a Brush Part Designed to Clean the Internal Channel of a Medical Device

$30.00 $60.00

ASTM A1025/A1025M-10(2020)

ASTM A1025/A1025M-10(2020)

Standard Specification for Ferroalloys and Other Alloying Materials, General Requirements

$22.00 $44.00