1.1 This practice is intended to assist electroplaters in establishing and maintaining a satisfactory pre-electroplating cycle for malleable iron, gray iron, nodular iron, and white iron castings. It is also intended to indicate certain foundry practices which will facilitate subsequent finishing. Most of the practices that follow have been based on experience with malleable and gray iron. However, since they are related to the other forms, the same practices will probably apply. Nodular iron is also known as spheroidal or ductile iron, which is defined as cast iron with the graphite substantially in spherical shape and substantially free of flake graphite.
1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 2.1.
Standard Test Method for Measuring Nitrogen Concentration in Silicon Substrates by Secondary Ion Mass Spectrometry (Withdrawn 2003)
$29.00 $58.00
Standard Test Method for Performance of Large Open Vat Fryers
$32.00 $65.00
Standard Guide for Construction of a Sounding Tube and Striker Plate for Tank Sounding
$25.00 $50.00
Standard Specification for Hand-Operated, Globe-Style Valves for Gas (Except Oxygen Gas), and Hydraulic Systems