1.1 This specification covers the requirements for 20 grades of titanium and titanium alloy tubing intended for surface condensers, evaporators, and heat exchangers, as follows:

1.1.1 Grade 1 - Unalloyed titanium,

1.1.2 Grade 2 - Unalloyed titanium,

1.1.3 Grade 3 - Unalloyed titanium,

1.1.4 Grade 7 - Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.5 Grade 9 - Titanium alloy (3 % aluminum, 2.5 % vanadium),

1.1.6 Grade 11 - Unalloyed titanium plus 0.12 to 0.25 % palladium,

1.1.7 Grade 12 - Titanium alloy (0.3 % molybdenum, 0.8 % nickel),

1.1.8 Grade 13 - Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.9 Grade 14 - Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.10 Grade 15 - Titanium alloy (0.5 % nickel, 0.05 % ruthenium),

1.1.11 Grade 16 - Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.12 Grade 17 - Unalloyed titanium plus 0.04 to 0.08 % palladium,

1.1.13 Grade 18 - Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.04 to 0.08 % palladium,

1.1.14 Grade 26 - Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.15 Grade 27 - Unalloyed titanium plus 0.08 to 0.14 % ruthenium,

1.1.16 Grade 28 - Titanium alloy (3 % aluminum, 2.5 % vanadium) plus 0.08 to 0.14 % ruthenium,

1.1.17 Grade 30 - Titanium alloy (0.3 % cobalt, 0.05 % palladium),

1.1.18 Grade 31 - Titanium alloy (0.3 % cobalt, 0.05 % palladium),

1.1.19 Grade 33 - Titanium alloy (0.4% nickel, 0.015% palladium, 0.025% ruthenium, 0.15% chromium), and

1.1.20 Grade 34 - Titanium alloy (0.4% nickel, 0.015% palladium, 0.025% ruthenium, 0.15% chromium).

1.1.21 Grade 35 - Titanium alloy (4.5 % aluminum, 2 % molybedenum, 1.6% vanadium, 0.5% iron, 0.3 % silicon).

1.2 Tubing covered by this specification shall be heat treated by at least a stress relief as defined in 5.3.

1.3 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.

More ASTM standard pdf

ASTM D8019-15

ASTM D8019-15

Standard Test Methods for Determining the Full Section Flexural Modulus and Bending Strength of Fiber Reinforced Polymer Crossarms Assembled with Center Mount Brackets

$24.00 $48.00

ASTM E1726-20

ASTM E1726-20

Standard Practice for Preparation of Soil Samples by Hotplate Digestion for Subsequent Lead Analysis

$32.00 $64.00

ASTM E1913-04(2012)

ASTM E1913-04(2012)

Standard Guide for Conducting Static, Axenic, 14-Day Phytotoxicity Tests in Test Tubes with the Submersed Aquatic Macrophyte, Myriophyllum sibiricum Komarov (Withdrawn 2012)

$32.00 $65.00

ASTM B42-15a

ASTM B42-15a

Standard Specification for Seamless Copper Pipe, Standard Sizes

$30.00 $60.00