• ASTM B408-06

ASTM B408-06

Standard Specification for Nickel-Iron-Chromium Alloy Rod and Bar

ASTM International, 12/01/2006

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:01/12/2006

Pages:5

File Size:1 file , 86 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers UNS N08120, UNS N08800, UNS N08810, UNS N08811*, and UNS N08890 in the form of hot-worked and cold-worked rod and bar. Alloy UNS N08800 is normally employed in service temperatures up to and including 1100F (593C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100F (593C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range.

1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.

More ASTM standard pdf

ASTM D3774-96(2008)e2

ASTM D3774-96(2008)e2

Standard Test Method for Width of Textile Fabric

$26.00 $52.00

ASTM F1657/F1657M-96(2012)e1

ASTM F1657/F1657M-96(2012)e1

Standard Practice for Emergency Joining of Booms with Incompatible Connectors

$25.00 $50.00

ASTM D5075-01(2007)

ASTM D5075-01(2007)

Standard Test Method for Nicotine and 3-Ethenylpyridine in Indoor Air

$30.00 $60.00

ASTM D1108-96(2007)

ASTM D1108-96(2007)

Standard Test Method for Dichloromethane Solubles in Wood

$26.00 $52.00