• ASTM B408-96

ASTM B408-96

Standard Specification for Nickel-Iron-Chromium Alloy Rod and Bar

ASTM International, 11/10/2001

Publisher: ASTM

File Format: PDF

$31.00$62.00


Published:10/11/2001

Pages:5

File Size:1 file , 29 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers UNS N08120, UNS N08800, UNS N08810, UNS N08811*, and UNS N08890 in the form of hot-worked and cold-worked rod and bar. Alloy UNS N08800 is normally employed in service temperatures up to and including 1100°F (593°C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100°F (593°C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range.

1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.

More ASTM standard pdf

ASTM E844-97

ASTM E844-97

Standard Guide for Sensor Set Design and Irradiation for Reactor Surveillance, E 706(IIC)

$29.00 $58.00

ASTM D6443-14

ASTM D6443-14

Standard Test Method for Determination of Calcium, Chlorine, Copper, Magnesium, Phosphorus, Sulfur, and Zinc in Unused Lubricating Oils and Additives by Wavelength Dispersive X-ray Fluorescence Spectrometry (Mathematical Correction Procedure)

$29.00 $58.00

ASTM D1196/D1196M-12(2016)

ASTM D1196/D1196M-12(2016)

Standard Test Method for Nonrepetitive Static Plate Load Tests of Soils and Flexible Pavement Components, for Use in Evaluation and Design of Airport and Highway Pavements

$27.00 $54.00

ASTM F853-04

ASTM F853-04

Standard Practice for Maintenance Procedures for Amusement Rides and Devices

$29.00 $58.00