1.1 This specification covers nickel-chromium-molybdenum-columbium alloys (UNS N06625 and UNS N06852) and nickel-chromium-molybdenum-silicon alloy (UNS N06219)* in the form of cold-worked seamless pipe and tube. The general requirements for pipe and tube are covered by Specification B 829.
1.1.1 UNS N06625 products are furnished in two grades of different heat-treated conditions:
Material is normally employed in service temperatures up to 1100F (593C).
Material is normally employed in service temperatures above 1100F (593C) when resistance to creep and rupture is required. Note 1
Hot-working or reannealing may change properties significantly, depending on working history and temperatures.
1.1.2 Alloys UNS N06219 and UNS N06852 are supplied in the solution annealed condition only.
The following precautionary caveat pertains only to the test methods portion, Section , of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.
Standard Guide for Selection of Test Methods for Ethylene Propylene Diene Terpolymer (EPDM) Geomembranes
$25.00 $50.00
Standard Test Method for Binding Sites Per Unit Length or Width of Pile Yarn Floor Coverings
$26.00 $52.00
Standard Practice for Installation of Water Vapor Retarders Used in Contact with Earth or Granular Fill Under Concrete Slabs
$29.00 $58.00
Standard Test Method for Softening Point of Pitches (Mettler Softening Point Method)
$30.00 $60.00