1.1''This guide describes two processes used for plating on magnesium and magnesium alloys: direct electroless nickel plating and zinc immersion. Some users report that the direct electroless nickel procedure does not produce quite as high a level of adhesion as zinc immersion.
1.2''The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.3''This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. For specific hazard statements, see 5.1.1 and 5.2.9.2.
1.4''This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
More ASTM standard pdf
ASTM G34-99
Standard Test Method for Exfoliation Corrosion Susceptibility in 2XXX and 7XXX Series Aluminum Alloys (EXCO Test)
$29.00 $58.00
ASTM D2305-99
Standard Test Methods for Polymeric Films Used for Electrical Insulation
$29.00 $58.00
ASTM E1384-99e1
Standard Guide for Content and Structure of the Electronic Health Record (EHR)
$60.00 $120.00