ASTM B591-08

Standard Specification for Copper-Zinc-Tin and Copper-Zinc-Tin-Iron-Nickel Alloys Plate, Sheet, Strip, and Rolled Bar

ASTM International, 04/01/2008

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:01/04/2008

Pages:6

File Size:1 file , 85 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers the requirements for specified copper-zinc-tin alloys and copper-zinc-tin-iron-nickel alloys in the form of plate, sheet, strip, and rolled bar. The alloys and nominal compositions are as follows:

Copper Alloy
UNS No.
Copper,
%
Tin,
%
Zinc,
%
Phos.,
%%
Iron,
%
Nickel,
%
C40500 95 1 4
C40810 95.5 2.0 2.22 0.03 0.1 0.15
C40850 95.5 3.0 1.27 0.1 0.1 0.1
C40860 94.8 2.0 3.04 0.03 0.03 0.1
C41100 91 0.5 8.5
C41300 91 1 8
C41500 91 2 7
C42200 87 1 12
C42500 88 2 10
C42520 89.8 2.0 7.97 0.1 0.1 0.1
C43000 85 2 13
C43400 85 0.7 14.3

1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

More ASTM standard pdf

ASTM B441-04

ASTM B441-04

Standard Specification for Copper-Cobalt-Beryllium, Copper-Nickel-Beryllium, and Copper-Nickel-Lead-Beryllium Rod and Bar (UNS Nos. C17500, C17510, and C17465)

$26.00 $52.00

ASTM D4363-98(2010)

ASTM D4363-98(2010)

Standard Specification for Thermoplastic Chlorinated Polyethylene (CM) Jacket for Wire and Cable

$26.00 $52.00

ASTM D3933-98(2010)

ASTM D3933-98(2010)

Standard Guide for Preparation of Aluminum Surfaces for Structural Adhesives Bonding (Phosphoric Acid Anodizing)

$30.00 $60.00

ASTM D4179-11

ASTM D4179-11

Standard Test Method for Single Pellet Crush Strength of Formed Catalysts and Catalyst Carriers

$26.00 $52.00