• ASTM B793-12

ASTM B793-12

Standard Specification for Zinc Casting Alloy Ingot for Sheet Metal Forming Dies and Plastic Injection Molds

ASTM International, 05/01/2012

Publisher: ASTM

File Format: PDF

$26.00$52.00


Published:01/05/2012

Pages:3

File Size:1 file , 71 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers commercial zinc alloys in ingot form for remelting for the manufacture of dies and molds from the alloys as shown in Table 1.

1.2 This specification presents requirements for zinc alloys suitable for the production of sand cast or plaster cast forming dies for sheet metal stamping operations and plastic injection molding. Alloy A is intended for use in the fabrication of dies for sheet metal stamping under drop hammer and hydraulic pressure. Alloy B is a special purpose alloy of closely controlled composition and is primarily used in the manufacture of plastic injection molds.

1.3 This specification covers two zinc alloys which are specified and designated as follows:

UNS ASTM Traditional
Z35543 Alloy A Kirksite A
Z35542 Alloy B Kirksite B

1.4 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use.

TABLE 1 Chemical and North American Color Code RequirementsA,B

Composition, %
UNS Z35543
Alloy A
Kirksite A
UNS Z35542
Alloy B
Kirksite B
Color CodeC Green/Red Green/Black
Element
Aluminum 3.5-4.5 3.9-4.3
Cadmium 0.005 max 0.003 max
Copper 2.5-3.5 2.5-2.9
Iron 0.100 max 0.075 max
Lead 0.007 max 0.003 max
Magnesium 0.02-0.10 0.02-0.05
Tin 0.005 max 0.001 max
Zinc Remainder Remainder

A The following applies to all specified limits in this table: For purposes of determining conformance with this specification, the observed value or calculated value obtained from analysis shall be rounded off "to the nearest unit" in the last right hand place of figures used in expressing the specified limit, in accordance with the rounding method of Practice E29.

B UNS designations were established in accordance with Practice E527.

C Refer to Practice B908. (Note: Colors indicated are for North American applications.)

More ASTM standard pdf

ASTM E1687-10(2014)

ASTM E1687-10(2014)

Standard Test Method for Determining Carcinogenic Potential of Virgin Base Oils in Metalworking Fluids

$30.00 $60.00

ASTM D5845-95(2000)e1

ASTM D5845-95(2000)e1

Standard Test Method for Determination of MTBE, ETBE, TAME, DIPE, Methanol, Ethanol and tert-Butanol in Gasoline by Infrared Spectroscopy

$29.00 $58.00

ASTM C170/C170M-14a

ASTM C170/C170M-14a

Standard Test Method for Compressive Strength of Dimension Stone

$25.00 $50.00

ASTM D6851-02(2011)

ASTM D6851-02(2011)

Standard Test Method for Determination of Contact pH with Activated Carbon

$26.00 $52.00