1.1 This specification covers procedures for reducing the susceptibility or degree of susceptibility to hydrogen embrittlement or degradation that may arise in the finishing processes.
1.2 The heat treatment procedures established herein have been shown to be effective for reducing susceptibility to hydrogen embrittlement. This heat-treatment procedure is used after plating operations but prior to any secondary conversion coating operation.
1.3 This specification has been coordinated with ISO/DIS 9588 and is technically equivalent.
Standard Test Method for Determination of Uranium Isotopic Composition by the Double Spike Method Using a Thermal Ionization Mass Spectrometer
$30.00 $60.00
Standard Test Method for Vapor Pressure of Petroleum Products and Liquid Fuels (Mini Method)
$28.00 $57.00
Standard Test Method for Determining Average Bonding Peel Strength Between Top and Bottom Layers of Needle-Punched Geosynthetic Clay Liners
$25.00 $50.00
Standard Test Method for Hydrogen Sulfide in Liquefied Petroleum (LP) Gases (Lead Acetate Method)