1.1 This specification covers high calcium, dolomitic and magnesian-hydrated lime for use in asphalt cement or bituminous pavement.
Note 1Hydrated lime, either calcitic, dolomitic, or magnesian, improves bonding of bitumen and aggregates which reduces susceptibility to moisture damage, reduces age hardening by chemically stabilizing polar compounds found in asphalts, and increases initial stiffness of asphalt mixtures.
Note 2No attempt is made to present requirements for any by-product lime.
This standard does not purport to address the safety concerns associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
More ASTM standard pdf
ASTM C1107-99
Standard Specification for Packaged Dry, Hydraulic-Cement Grout (Nonshrink)
$29.00 $58.00
ASTM C633-79(1999)
Standard Test Method for Adhesion or Cohesion Strength of Thermal Spray Coatings
$29.00 $58.00
ASTM A798/A798M-01
Standard Practice for Installing Factory-Made Corrugated Steel Pipe for Sewers and Other Applications
$30.00 $60.00