1.1 This practice provides one environment in which to expose finished pressure-sensitive tape material for the purpose of accelerating the aging of it. It is applicable to tape in roll form when the user observes the precautions detailed within the procedure. The practice does not provide for a conclusion within itself, but is for use in conjunction with appearance or physical property tests to follow the accelerated exposure. While this practice was developed using packaging type tapes, its use on other types of tape with similar construction is encouraged. It is not intended for use on electrical grade tapes (see Test Methods D1000).
1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Specification for Aluminum-Coated Steel Chain-Link Fence Fabric
$27.00 $54.00
Standard Test Methods for Nitrogen in the Analysis Sample of Refuse-Derived Fuel
$29.00 $58.00
Standard Test Method for Determination of Crushing Strength of Iron Ore Pellets
$26.00 $52.00
Terminology Relating to Thermometry and Hydrometry
$33.00 $67.00