1.1 This test method covers the procedure for distillation of heavy hydrocarbon mixtures having initial boiling points greater than 150°C (300°F), such as heavy crude oils, petroleum distillates, residues, and synthetic mixtures. It employs a potstill with a low pressure drop entrainment separator operated under total takeoff conditions. Distillation conditions and equipment performance criteria are specified and typical apparatus is illustrated.

1.2 This test method details the procedures for the production of distillate fractions of standardized quality in the gas oil and lubricating oil range as well as the production of standard residua. In addition, it provides for the determination of standard distillation curves to the highest atmospheric equivalent temperature possible by conventional distillation.

1.3 The maximum achievable atmospheric equivalent temperature (AET) is dependent upon the heat tolerance of the charge. For most samples, a temperature up to 565°C (10570°F) can be attained. This maximum will be significantly lower for heat sensitive samples (for example, heavy residues) and might be somewhat higher for nonheat sensitive samples.

1.4 The recommended distillation method for crude oils up to cutpoint 400°C (752°F) AET is Test Method D 2892. This test method can be used for heavy crude oils with initial boiling points greater than 150 - C (302°F). However, distillation curves and fraction qualities obtained by these methods are not comparable.

1.5 This test method contains the following annexes:

1.5.1 Annex A1 - Test Method for Determination of the Temperature Response Time,

1.5.2 Annex A2 - Practice for Calibration of Sensors,

1.5.3 Annex A3 - Test Method for Dehydration of a Wet Sample of Oil,

1.5.4 Annex A4 - Practice for Conversion of Observed Vapor Temperature to Atmospheric Equivalent Temperature (AET), and

1.5.5 Annex A5 - Test Method for Determination of Wettage.

1.6 The values stated in SI units are to be regarded as the standard. The inch-pound units given in parentheses are provided for information purposes only.

1.7 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. For specific warnings see 6.5.4.2, 6.5.6.3, 6.9.3, 9.5, 9.6 and A2.3.1.3.

More ASTM standard pdf

ASTM C443-19

ASTM C443-19

Standard Specification for Joints for Concrete Pipe and Manholes, Using Rubber Gaskets

$29.00 $58.00

ASTM C1334-05(2022)

ASTM C1334-05(2022)

Standard Specification for Uranium Oxides with a 235U Content of Less Than 5 % for Dissolution Prior to Conversion to Nuclear-Grade Uranium Dioxide

$24.00 $48.00

ASTM D6905-20

ASTM D6905-20

Standard Practice for Impact Flexibility of Organic Coatings

$23.00 $46.00

ASTM B719-20

ASTM B719-20

Standard Specification for Nickel-Chromium-Molybdenum-Cobalt-Tungsten-Iron-Silicon Alloy Bar

$25.00 $50.00