• ASTM D5419-09

ASTM D5419-09

Standard Test Method for Environmental Stress Crack Resistance (ESCR) of Threaded Plastic Closures

ASTM International, 11/15/2009

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:15/11/2009

Pages:5

File Size:1 file , 120 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This test method determines the susceptibility of threaded plastic closures to failure due to environmental stress cracking (ESC).

1.2 In use, threaded plastic closures can contact agents that appreciably reduce the stress at which cracks form. Examples of such agents are: soaps, detergents, oils, and liquid bleaches.

1.3 Major factors that influence environmental stress crack resistance (ESCR) of threaded plastic closures include the closure material(s), closure design, molded-in stress, and applied stress.

1.4 This procedure can be applied to all closures, but is particularly applicable to closures made from plastics based on polypropylene (PP) or polystyrene (PS).

1.5 The values stated in SI units are to be regarded as the standard.

1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 8 and 6.2.

Note 1 - There is no known ISO equivalent to this test method.

More ASTM standard pdf

ASTM C1053-00(2010)

ASTM C1053-00(2010)

Standard Specification for Borosilicate Glass Pipe and Fittings for Drain, Waste, and Vent (DWV) Applications

$33.00 $67.00

ASTM D7124-17

ASTM D7124-17

Standard Specification for Benzene for Use with Zeolite Based Catalysts

$26.00 $52.00

ASTM D5770-02

ASTM D5770-02

Standard Test Method for Semiquantitative Micro Determination of Acid Number of Lubricating Oils During Oxidation Testing

$26.00 $52.00

ASTM D4576-86(1996)

ASTM D4576-86(1996)

Standard Test Method for Mold Growth Resistance of Wet Blue

$25.00 $50.00