1.1 This test method covers the preparation and testing of thick-adherend lap-shear samples for the determination of the stress-strain behavior of adhesives.
1.2 This test method covers data reduction and analysis of stress-strain curves obtained using thick-adherend lap-shear samples.
1.3 The values stated in SI units are to be regarded as the standard. The inch-pound units in parentheses are for information only.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 7.3.
Standard Practice for Determining Damage-Based Design Stress for Glass Fiber Reinforced Plastic (GFRP) Materials Using Acoustic Emission
$34.00 $68.00
Standard Test Method for Freeze/Thaw Resistance of Wax Emulsion Floor Polish
$30.00 $60.00
Standard Test Method for Peel Adhesion of Pressure-Sensitive Tape
$26.00 $52.00
Standard Practice for Testing Engine Coolants in Car and Light Truck Service
$25.00 $50.00