ASTM International, 11/01/2012
Publisher: ASTM
File Format: PDF
$30.00$60.00
Published:01/11/2012
Pages:6
File Size:1 file , 100 KB
Note:This product is unavailable in Russia, Ukraine, Belarus
1.1 This test method is used for the determination of free formaldehyde (HCHO) in emulsion polymers without upsetting existing formaldehyde equilibria. The procedure has been evaluated using acrylic, acrylonitrile-butadiene, carboxylated styrene-butadiene and polyvinyl acetate emulsion polymers. This test method may also be applicable for emulsion polymers of other compositions. The established working range of this test method is from 0.05 to 15 ppm formaldehyde. Emulsion polymers must be diluted to meet the working range.
1.2 This test method minimizes changes in free formaldehyde concentration that can result from changes in the physical or chemical properties of an emulsion polymer.
1.3 There are no known limitations to this test method when used in the manner described. The emulsion polymer test specimen must be prepared with a diluent that has a pH similar to that of the emulsion. Use of an inappropriate pH may upset formaldehyde equilibria and result in incorrect formaldehyde levels.
1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Practice for Use of Hydraulic Cement Mortars in Chemical-Resistant Masonry
$26.00 $52.00
Standard Specification for Technical Grade Ethylene Dichloride
Standard Test Method for Thermal Stability Testing of Gallium Arsenide Wafers (Withdrawn 2008)
$25.00 $50.00
Standard Test Method for Tensile Properties of Paper and Paperboard Using Constant-Rate-of-Elongation Apparatus
$30.00 $60.00