1.1 This practice covers determination of glass transition temperatures of hydrocarbon (HC) resins by differential scanning calorimetry (DSC).
1.2 This practice is applicable to HC resins as defined in Terminology D 6440. The normal operating temperature range is from the cryogenic region to approximately 180°C. The temperature range can be extended.
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 Further discussion of glass transition can be found in Test Method D 3418, and Test Method E 1356.
1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Test Method for Density of Adhesives in Fluid Form
$17.00 $35.00
Standard Test Method for Pyridine Bases in Cresylic Acid by Direct Titration
$26.00 $52.00
Standard Specification for Reference Masses and Devices for Determining Mass and Volume for Use in the Physical Testing of Hydraulic Cements
Standard Test Methods for Physical Testing of Quicklime, Hydrated Lime, and Limestone
$43.00 $86.00