1.1 This practice covers determination of glass transition temperatures of hydrocarbon (HC) resins by differential scanning calorimetry (DSC).
1.2 This practice is applicable to HC resins as defined in Terminology D6640. The normal operating temperature range is from the cryogenic region to approximately 180°C. The temperature range can be extended.
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 Further discussion of glass transition can be found in Test Method D3418, and Test Method E1356.
1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Test Method for Absorption of Architectural Cast Stone
$27.00 $54.00
Standard Specification for Marble Dimension Stone
$26.00 $52.00
Standard Test Method for Compressive Residual Strength Properties of Damaged Polymer Matrix Composite Plates
$33.00 $67.00
Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes