1.1 These test methods cover the determination of total iron in iron ores, concentrates, and agglomerates in the concentration range 30 % to 95 % iron.
1.2 The test methods in this standard are contained in the sections indicated as follows:
Test Method A- Iron by the Hydrogen Sulfide Reduction Dichromate Titration Method (30 % to 75 % Fe)
Test Method B-Iron by the Stannous Chloride Reduction Dichromate Titration Method (35 % to 95 % Fe)
Test Method C-Iron by the Silver Reduction Dichromate Titration Method (35 % to 95 % Fe)
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific hazards statements are given in Section 5 and in special “Warning” paragraphs throughout these test methods.
Standard Specification for Dimensional Tolerance of Thermosetting Glass-Reinforced Plastic Pultruded Shapes
$30.00 $60.00
Standard Test Method for Torsional Ring Shear Test to Determine Drained Residual Shear Strength of Cohesive Soils
Standard Test Method for Evaporation Loss of Lubricating Oils by Thermogravimetric Analyzer (TGA) Noack Method
Standard Test Method for Electrochemical Measurement of Diffusible Hydrogen in Steels (Barnacle Electrode)
$29.00 $58.00