1.1 This test method is used to determine the susceptibility of high-density polyethylene (HDPE) resins or corrugated pipe to slow-crack-growth under a constant ligament-stress in an accelerating environment. This test method is intended to apply only to HDPE of a limited melt index and density range as defined in AASHTO Standard Specification M 294. This test method may be applicable for other materials, but data are not available for other materials at this time.
1.2 This test method measures the failure time associated with a given test specimen at a constant, specified, ligament-stress level.
1.3 The values stated in inch-pound units are to be regarded as the standard. Values given in parentheses are for information only.
1.4 Definitions are in accordance with Terminology F 412, and abbreviations are in accordance with Terminology D 1600, unless otherwise specified.
1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Test Method for Corrosiveness to Silver by Automotive Spark-Ignition Engine Fuel-Silver Strip Method
$30.00 $60.00
Standard Specification for High-Strength Quenched and Tempered Low-Alloy Steel Forged Fittings and Parts for Pressure Vessels
$26.00 $52.00
Standard Specification for Wrought Austenitic Stainless Steel Piping Fittings
Standard Practice for Evaluation of Image Quality Produced by Carbonless Copy Paper with an Electric or Electronic Typewriter (Withdrawn 2020)