1.1 This test method covers the use of the subthreshold charge separation technique for analysis of ionizing radiation degradation of a gate dielectric in a metal-oxide-semiconductor-field-effect transistor (MOSFET) and an isolation dielectric in a parasitic MOSFET. , , The subthreshold technique is used to separate the ionizing radiation-induced inversion voltage shift, ΔVINV into voltage shifts due to oxide trapped charge, ΔVot and interface traps, ΔVit. This technique uses the pre- and post-irradiation drain to source current versus gate voltage characteristics in the MOSFET subthreshold region.
1.2 Procedures are given for measuring the MOSFET subthreshold current-voltage characteristics and for the calculation of results.
1.3 The application of this test method requires the MOSFET to have a substrate (body) contact.
1.4 Both pre- and post-irradiation MOSFET subthreshold source or drain curves must follow an exponential dependence on gate voltage for a minimum of two decades of current.
1.5 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Standard Specification for Calcium Chloride
$25.00 $50.00
Standard Test Method for Laboratory Measurement of Impact Sound Transmission Through Floor-Ceiling Assemblies Using the Tapping Machine
$30.00 $60.00
Standard Practice for Rubber - ;Chromatographic Analysis of Antidegradants (Antioxidants, Antiozonants and Stabilizers)
$31.00 $62.00
Standard Practice for Fabricating Ceramic Reference Specimens Containing Seeded Voids