• BS 3HR 2:2010+A1:2011

BS 3HR 2:2010+A1:2011

Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

BSI Group, 01/31/2010

Publisher: BS

File Format: PDF

$60.00$121.92


Published:31/01/2010

Pages:16

File Size:1 file , 2.1 MB

Note:This product is unavailable in Ukraine, Russia, Belarus



Cross References:
BS HR 100
EN 4500-1
EN 4500-3


Incorporates the following:
Amendment, January 2011. Amends and replaces BS 3HR 2:2010

More BS standard pdf

BS 96/716608 DC

BS 96/716608 DC

Aerospace series. Heat resisting alloy NI-PD9201 (NiCu31) annealed. Seamless tube D < 75 mm - 3 < 3 mm (prEN 4373)

$126.00 $252.88

BS 96/716615 DC

BS 96/716615 DC

Aerospace series. Heat resisting alloy NI-PH3601 (NiCr22Mo9Nb) solution treated. Bar and section a or D < 200 mm (prEN 4380)

$118.00 $236.18

BS 96/717410 DC

BS 96/717410 DC

Aerospace series. Heat resisting alloy FE-PA2602 (X4NiCrTiMoV26-15) solution and precipitation treated. Bar and section a or D < 100 mm (prEN 3510)

$104.00 $208.94

BS 96/716603 DC

BS 96/716603 DC

Aerospace series. Heat resisting alloy NI-CD1701 (NiCo15Cr10A16Ti5Mo3) as cast. Remelting stock (prEN 4368)

$133.00 $266.41