• BS 6721-9:1989

BS 6721-9:1989

Sampling and analysis of copper and copper alloys-Method for determination of lead in copper alloys by flame atomic absorption spectrophotometry

BSI Group, 02/28/1989

Publisher: BS

File Format: PDF

$76.00$152.40


Published:28/02/1989

Pages:8

File Size:1 file , 650 KB

Note:This product is unavailable in Ukraine, Russia, Belarus

Lead content between 0.01 and 5.0% (m/m) in copper and copper alloys. The lower limit may be extended to 0.002% (m/m) by using a smaller sample mass.

More BS standard pdf

BS TA 42:1971

BS TA 42:1971

Specification for forgings of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1205-1375 N/mm2) (limiting ruling section over 25 mm up to and including 75 mm)

$76.00 $152.40

BS L 112:1971

BS L 112:1971

Specification for forging stock and forgings of aluminium-magnesium-silicon-manganese alloy (solution treated and precipitation treated) (suitable for welding) (Mg 0.8, Si 1, Mn 0.7)

$76.00 $152.40

BS 4770:1971

BS 4770:1971

Specification for bunched enamelled copper conductors with silk covering

$125.00 $251.46

BS TA 41:1971

BS TA 41:1971

Specification for forging stock of titanium-aluminium-molybdenum-tin-silicon-carbon alloy (tensile strength 1205-1375 N/mm2) (limiting ruling section over 25 mm up to and including 75 mm)

$76.00 $152.40