This standard describes a test method to measure specific physical properties and the relative stability of Cu/CuSO4 PREs when they are subjected to specific environmental stresses. These reference electrodes, while "permanent" in the physical sense (they are not commonly removed), do exhibit a finite service life. This test method is intended to provide a measure of the relative durability that may be expected. This standard is maintained by Task Group 256.

More NACE standard pdf

NACE SP0106-2006

NACE SP0106-2006

Control of Internal Corrosion in Steel Pipelines and Piping Systems

$89.00 $179.00

NACE SP0294-2006

NACE SP0294-2006

Standard Practice - Design, Fabrication, and Inspection of Storage Tank Systems for Concentrated Fresh and Process Sulfuric Acid and Oleum at Ambient Temperatures

$89.00 $179.00

NACE SP0206-2006

NACE SP0206-2006

Internal Corrosion Direct Assessment Methodology for Pipelines Carrying Normally Dry Natural Gas (DG-ICDA)

$89.00 $179.00

NACE No. 8/SSPC-SP 14

NACE No. 8/SSPC-SP 14

Joint Surface Preparation Standard - Industrial Blast Cleaning

$89.00 $179.00